About UNINAKS

Products

Manuals

PLOCK ADHESIVE

FIRE-RESISTANT MASONRY MORTAR

GYPSUM PLASTER

SILER-4

FIBRE PLASTER

LIME MORTAR

MÜÜRISEGU M 100

MÜÜRISEGU M 200

NAKS-4

TELLISESILER

CAST CONCRETE M 300

FIBRE-CONCRETE

SELF-STRESSING CONCRETE M 400

GRANIT CONCRETE M 500

VERTICAL JOINTING CONCRETE

FIRE CONCRETE

MARBLE CONCRETE

COCRETE C30

NON-SHRINK CONCRETE C70

KIUDKROHV

MORTAR-STONE ADHESIVE "MÜÜRIMÖRT"

NAKS+P

NOBENAKS

PÕRANDANAKS

CLAY PLASTER

QUICK SET CONCRETE

UniTherm INSULATION BONDING MIX

UniTherm ARMOURING GLUE

UniTherm STRUCTURAL PLASTER

UniTherm DEEP IMPREGNATING PRIMING COAT

MASONRY MORTAR FOR REFRACTORY BRICKS

Contacts

ISO 9001:2008 Certificate

Certificate of Factory Product Control

EU Declarations of Conformity

Color palet

TALLINN
müügiesindus ja ladu

Forelli 11, Tallinn 10621
Tel/faks.: 65 65 744
E-mail: uninaks[at]uninaks.ee

LIHULA
tehas, müük ja ladu

Valuste tee 1, Lihula 90303
Tel/faks: 47 78 743

SIA UNINAKS LATVIJA

Katlakalna ielā 11C, Riga, Latvija
Schenker noliktavās
Tel/Fax: +371 67 544 085
E-mail: uninaks[at]inbox.lv







WHITE POLYMER CONCRETE FOR MINOR CASTING WORKS

MARBLE CONCRETE

COMPRESSIVE STRENGTH CLASS C35/45 EVS-EN 206-1:2007

 

For concrete casting works of decorative nature.

FOR CASTING SMALLER CONCRETE ELEMENTS

 

SUITABLE FOR INTERNAL AND EXTERNAL WORKS.

 

COMPOSITION

White lime gravel (max. grain size 3 mm), light quartz sand, white cement 52.5 N, polymers and plasticisers.

 

PREPARATION FOR USE

Pour necessary amount of powder into a suitable container or mixer.

Add water in the amount of 13-15% of powder weight. (3.25-3.75 litres for 25 kg bag)

Stir mechanically or manually until the compound is fully homogenous.

Let the mix settle for a while and stir once again.

Use the prepared mix within 2 hours.

 

TECHNICAL SPECIFICATIONS

Compressive strength class of hardened concrete: C35/45 EVS-EN 206-1:2002

25 kg of dry concrete makes approx. 12 litres of the ready mix.

Concrete hardening in temperature conditions of +200 C shall develop the following approximate strength values:

7 days           35 MPa

28 days            over 45 MPa

Marble concrete has higher weather resistance and surface hardening factor thanks to polymeric additives in the mix.

NB ! Lower temperatures slow down hardening speed of concrete.

 

LIMITATIONS – WARNINGS

Substrate and ambient temperature during the application process shall exceed zero. Avoid freezing of the freshly poured concrete.

Drying fresh surfaces shall be protected from rain and direct sunlight exposure. If necessary use water to moisten freshly poured concrete.

The product contains cement. Contact with water causes alkaline reaction. Can cause skin irritation. Upon contact with eyes rinse immediately with plenty of fresh water. For more specific information please refer to the Safety Data Sheet.

 

STORAGE

Bagged mix powder has to be stored in dry conditions.

Shelf life is 1 year.